10-32"0.34400.28500.1510
1/4"0.43700.34000.1820
5/16"0.50000.41000.2320
3/8"0.56200.49000.2920
7/16"0.68700.57000.3570
1/2"0.75000.66000.4200
9/16"0.87500.72500.4830
5/8"0.93700.81000.5450
3/4"1.12500.97500.6700
7/8"1.31201.05100.7030
1"1.50001.18500.7920
1.1/8"1.68701.35800.8700
1.1/4"1.87501.49800.9600
1.3/8"2.06201.64601.0550
1.1/2"2.25001.79901.1500
1.3/4"2.62502.10101.3650
2"3.00002.22601.4250
2.1/4"3.75502.34001.5100
2.1/2"3.75002.55001.6850
2.3/4"4.12502.84501.9300
3"4.50003.06202.1500
Additional Info
Additional Info
Weight0.0000
MaterialClass-8
Standard Number.
Second StandardPHILIDAS
DriveHexagon
HeadNON
American Generic Brand Term STIFF, PREVAILING TORQUE
Diameter 10-32",1/4",5/16",3/8",7/16",1/2",9/16",5/8",3/4",7/8",1",1.1/8",1.1/4",1.3/8",1.1/2",1.3/4",2",2.1/4",2.1/2",2.3/4",3"
LengthNON
Reviews
Tags
Tags

Use spaces to separate tags. Use single quotes (') for phrases.