Smalley Crest to Crest Wave Spring Inch Stainless Steel

SKU: 2442
Details
Details

Smalley Crest to Crest Wave Spring Inch Stainless Steel

 

 

  • Wave springs reduce spring height by 50%
  • Same force and deflection as ordinary coil / compression springs
  • Wave springs fit tight radial and axial spaces 
  • Over 4,000 standard springs in carbon and stainless steel (¼" to 16", 6 mm to 400 mm) 
  • No Tooling Charges™ on custom designs (.200" to 120" diameters) 
  • Exotic alloys available

Smalley Wave Springs (Flat Wire Compression Springs) offer the unique advantage of space savings when used to replace coil springs. By reducing spring operating height, wave springs also produce a decrease in the spring cavity. With a smaller assembly size and less material used in the manufacturing process, a cost savings is realized.

Wave springs operate as load bearing devices. They take up play and compensate for dimensional variations within assemblies. A virtually unlimited range of forces can be produced whereby loads build either gradually or abruptly to reach a predetermined working height. This establishes a precise spring rate in which load is proportional to deflection.

Functional requirements are necessary for both dynamic and static spring applications. Special performance characteristics are individually built into each spring to satisfy a variety of precise operating conditions. Typically, a wave spring will occupy an extremely small area for the amount of work it performs. The use of this product is demanded, but not limited to tight axial and radial space constraints.

Part Number Operates in a bore dia.  Clears Shaft dia. Load (lb) Work Height  Reference Free Height No of WavesNo of Turns Thickness  Radial Wall Reference Spring Rate (lb/in)
YC025-L1* S17       0.250       0.1502       0.033       0.0752.53       0.006       0.02448
YC025-L2* S17       0.250       0.1502       0.050       0.1002.54       0.006       0.02440
YC025-L3* S17       0.250       0.1502       0.060       0.1252.55       0.006       0.02431
YC025-L4* S17       0.250       0.1502       0.075       0.1502.56       0.006       0.02427
YC025-L5* S17       0.250       0.1502       0.085       0.1752.57       0.006       0.02422
YC025-L6* S17       0.250       0.1502       0.095       0.2002.58       0.006       0.02419
YC025-L7* S17       0.250       0.1502       0.120       0.2252.59       0.006       0.02419
YC025-L8* S17       0.250       0.1502       0.140       0.2752.511       0.006       0.02415
YC025-L9* S17       0.250       0.1502       0.170       0.3252.513       0.006       0.02413
YC025-M1* S17       0.250       0.1505       0.037       0.0752.53       0.008       0.024132
YC025-M2* S17       0.250       0.1505       0.048       0.1002.54       0.008       0.02496
YC025-M3* S17       0.250       0.1505       0.065       0.1252.55       0.008       0.02483
YC025-M4* S17       0.250       0.1505       0.075       0.1502.56       0.008       0.02467
YC025-M5* S17       0.250       0.1505       0.090       0.1752.57       0.008       0.02459
YC025-M6* S17       0.250       0.1505       0.100       0.2002.58       0.008       0.02450
YC025-M7* S17       0.250       0.1505       0.120       0.2252.59       0.008       0.02448
YC025-M8* S17       0.250       0.1505       0.148       0.2752.511       0.008       0.02439
YC025-M9* S17       0.250       0.1505       0.175       0.3252.513       0.008       0.02433
YC031-L1 S17       0.312       0.2003       0.070       0.1142.53       0.008       0.03268
YC031-L2 S17       0.312       0.2003       0.096       0.1522.54       0.008       0.03254
YC031-L3 S17       0.312       0.2003       0.118       0.1902.55       0.008       0.03242
YC031-L4 S17       0.312       0.2003       0.145       0.2282.56       0.008       0.03236
YC031-L5 S17       0.312       0.2003       0.165       0.2662.57       0.008       0.03230
YC031-L6 S17       0.312       0.2003       0.195       0.3042.58       0.008       0.03228
YC031-L7 S17       0.312       0.2003       0.215       0.3422.59       0.008       0.03224
YC031-L8 S17       0.312       0.2003       0.262       0.4182.511       0.008       0.03219
YC031-L9 S17       0.312       0.2003       0.309       0.4942.513       0.008       0.03216
YC031-M1 S17       0.312       0.2006       0.072       0.1142.53       0.010       0.032143
YC031-M2 S17       0.312       0.2006       0.096       0.1522.54       0.010       0.032107
YC031-M3 S17       0.312       0.2006       0.123       0.1902.55       0.010       0.03290
YC031-M4 S17       0.312       0.2006       0.144       0.2282.56       0.010       0.03271
YC031-M5 S17       0.312       0.2006       0.176       0.2662.57       0.010       0.03267
YC031-M6 S17       0.312       0.2006       0.197       0.3042.58       0.010       0.03256
YC031-M7 S17       0.312       0.2006       0.227       0.3422.59       0.010       0.03252
YC031-M8 S17       0.312       0.2006       0.278       0.4182.511       0.010       0.03243
YC031-M9 S17       0.312       0.2006       0.336       0.4942.513       0.010       0.03238
YC037-L1 S17       0.375       0.2504       0.062       0.1502.53       0.008       0.03245
YC037-L2 S17       0.375       0.2504       0.098       0.2002.54       0.008       0.03239
YC037-L3 S17       0.375       0.2504       0.108       0.2502.55       0.008       0.03228
YC037-L4 S17       0.375       0.2504       0.135       0.3002.56       0.008       0.03224
YC037-L5 S17       0.375       0.2504       0.150       0.3502.57       0.008       0.03220
YC037-L6 S17       0.375       0.2504       0.184       0.4002.58       0.008       0.03219
YC037-L7 S17       0.375       0.2504       0.195       0.4502.59       0.008       0.03216
YC037-L8 S17       0.375       0.2504       0.228       0.5002.510       0.008       0.03215
YC037-L9 S17       0.375       0.2504       0.240       0.5502.511       0.008       0.03213
YC037-M1 S17       0.375       0.2507       0.081       0.1502.53       0.011       0.032101
YC037-M2 S17       0.375       0.2507       0.119       0.2002.54       0.011       0.03286
YC037-M3 S17       0.375       0.2507       0.145       0.2502.55       0.011       0.03267
YC037-M4 S17       0.375       0.2507       0.180       0.3002.56       0.011       0.03258
YC037-M5 S17       0.375       0.2507       0.202       0.3502.57       0.011       0.03247
YC037-M6 S17       0.375       0.2507       0.240       0.4002.58       0.011       0.03244
YC037-M7 S17       0.375       0.2507       0.262       0.4502.59       0.011       0.03237
YC037-M8 S17       0.375       0.2507       0.298       0.5002.510       0.011       0.03235
YC037-M9 S17       0.375       0.2507       0.327       0.5502.511       0.011       0.03231
Additional Info
Additional Info
Weight0.0100
Material0
Standard NumberNo
Second StandardNo
Drive0
Head -
American Generic Brand TermNo
Diameter0
LengthNo
Reviews
Tags
Tags

Use spaces to separate tags. Use single quotes (') for phrases.