Metric Sealing Washer Aluminium DIN7603A

SKU: 1555
Details
Details
Metric Sealing Washer Aluminium DIN7603A
D d1 d2 h
M66.000012.00001.0000
M88.000012.00001.0000
M1010.000014.00001.0000
M1212.000016.00001.5000
M1414.000018.00001.5000
M1616.000022.00001.5000
M1818.000024.00001.5000
M2222.000027.00001.5000
Additional Info
Additional Info
Weight0.0000
MaterialALUMINIUM
Standard NumberDIN7603A
Second Standard-
DriveNon
HeadNON
American Generic Brand Term-
Diameter M6,M8,M10,M12,M14,M16,M18,M22