dadadkkcrrfyCyFl minl max
ST 2.91.10003.50007.50002.35000.80000.10003.80002.60002.10006.500019.0000
ST 3.51.30004.10009.00002.60000.90000.10004.60003.20002.50009.500025.0000
ST 4.21.40004.900010.00003.05001.10000.20005.80003.70002.80009.500032.0000
ST 4.81.60005.600011.50003.55001.35000.20006.60004.30003.20009.500038.0000
ST 5.51.80006.300013.00003.80001.60000.25007.80005.00003.600013.000038.0000
ST 6.31.80007.300014.50004.55001.80000.25008.20006.00003.600013.000038.0000
Additional Info
Additional Info
Weight0.0000
MaterialCASE HARDENED STEEL
Standard NumberDIN968FZ
Second Standard-
DrivePOZI,CROSSRECESSED
HeadFlangepan
American Generic Brand Term-
Diameter ST2.9,ST3.5,ST4.2,ST4.8,ST5.5,ST6.3
Length6.5,9.5,13,19,25,32,38