Metric Coarse Wing Nut Type A Usa Type CF British Steel Cold Forged DIN314AF

SKU: 1131
Details
Details
Metric Coarse Wing Nut Type A Usa Type CF British Steel Cold Forged DIN314AF
dh maxh minm maxm mind1 mind1 maxe maxe ming
?411.00009.00004.60003.20007.00009.000021.000019.00001.1000
?513.000011.00006.00004.00009.000012.000026.500024.50001.5000
M616.000014.00007.00005.000011.000014.000032.000029.00001.5000
M819.000017.00008.50006.500013.000016.000038.000035.00002.0000
M1024.000022.000010.00008.000018.000021.000050.000047.00003.6000
M1232.000029.000013.000010.000021.000024.000066.000063.00004.1000
Additional Info
Additional Info
Weight0.0000
MaterialSTEEL COLD FORGED
Standard NumberDIN314AF
Second Standard-
DriveWing
HeadNON
American Generic Brand TermTHUMB
Diameter ?4,?5,M6,M8,M10,M12