Metric Coarse Socket Cap Screw Grade-12.9 DIN912

SKU: 1618
Details
Details

Metric Coarse

Socket Cap Screw 12.9 DIN912

 

Dsdk Maxdk Mink Maxk Mintb
M1.4    1.302.742.461.401.260.60 14.00
M1.61.503.142.861.601.460.7015.00
M21.503.983.622.001.881.0016.00
M2.52.004.684.322.502.361.1017.00
M32.505.685.323.002.861.3018.00
M3.52.506.005.643.503.361.6020.00
M43.007.226.784.003.822.0020.00
M54.008.728.285.004.822.5022.00
M65.0010.229.786.005.703.0024.00
M86.0013.2712.738.007.644.0028.00
M108.0016.0016.2710.009.645.0032.00
M1210.0018.0018.2712.0011.576.0036.00
M1412.0021.0021.3314.0013.577.0040.00
M1614.0024.0024.3316.0015.578.0044.00
M1814.0027.0027.3318.0017.579.0048.00
M2017.0030.0030.3320.0019.4810.0052.00
M2217.0033.0033.3922.0021.4811.0056.00
M2419.0036.0036.3924.0023.4812.0060.00
M2719.0040.0040.3927.0026.4813.2066.00
M3022.0045.0045.3930.0029.4815.5072.00
M3324.0050.3949.6133.0032.3818.0078.00
M3627.0054.4653.5436.0035.3819.0084.00
M4232.0063.4662.5442.0041.3724.0096.00
M4836.0072.4671.5448.0047.3828.00108.00
M5641.0084.5483.4656.0056.2634.00124.00
M6446.0096.5495.4664.0063.2638.00140.00
M7255.00108.54107.4672.0071.2643.00156.00
M8065.00120.54119.4680.0079.2648.00172.00
M9075.00135.63134.3790.0089.1354.00192.00
M10085.00150.63149.37100.0099.1360.00212.00

 Metric Coarse Socket Cap Screw Grade class 12.9 DIN 912 allen

Additional Info
Additional Info
Weight0.0000
MaterialGrade-12.9
Standard NumberDIN 912
Second StandardBS4168,ISO4762
DriveHexagonsocket
HeadCAP
American Generic Brand TermALLEN
Diameter M1.6,M2,M2.5,M3,M3.5,M4,M5,M6,M7,M8,M10,M12,M14,M16,M18,M20,M22,M24,M27,M30,M33,M36,M39,M42,M45,M48,M52,M56,M60,M64,M68,M72,M76,M80,M90,M100,M110,M125,M140,M160
Length6,8,10,12,14,16,18,20,22,24,26,28,30,35,40,45,50,55,60,65,70,75,80,85,90,95,100,110,120,130,140,150,160,170,180,190,200,210,220,230,240,250,260,270,280,300,320,340,350,360,380,400,420,440,460,480,500
Reviews
Tags
Tags

Use spaces to separate tags. Use single quotes (') for phrases.