Metric Coarse Hexagon Head Bolt Grade-12.9 DIN931

SKU: 3
Details
Details

 

Dk nomk MaxMins maxs mine nome MaxMin
M1.61.10001.22500.97503.20003.08003.41003.70003.4800
M21.40001.52501.27504.00003.88004.32004.60004.3800
M2.51.70001.82501.57505.00004.88005.45005.80005.5100
M32.00002.12501.87505.50005.38006.01006.40006.0800
M3.52.4000  6.0000 6.5800  
M42.80002.92502.67507.00006.85007.66008.10007.7400
M53.50003.65003.35008.00007.85008.79009.20008.8700
M64.00004.15003.850010.00009.780011.050011.500011.0500
M74.8000  11.0000 12.1200  
M85.30005.65005.350013.000012.730014.380015.000014.3800
M106.40007.18006.820017.000016.730018.900019.600018.9000
M127.50008.18007.820019.000018.670021.100021.900021.1000
M148.80009.18008.820022.000021.670024.490025.400024.4900
M1610.000010.18009.820024.000023.670026.750027.700026.7500
M1811.500012.215011.785027.000026.670030.140031.200030.1400
M2012.500013.215012.785030.000029.670033.530034.600033.5300
M2214.000014.215013.785032.000031.610035.720036.900035.7200
M2415.000015.215014.785036.000035.380039.980041.600039.9800
M2717.000017.215016.785041.000040.380045.200047.300045.6300
M3018.700019.260018.740046.000045.380050.850053.100051.2800
M3321.000021.260020.740050.000049.380055.370057.700055.8000
M3622.500023.260022.740055.000054.260060.790063.500061.3100
M3925.000025.260024.740060.000059.260066.400069.300066.9600
M4226.000026.260025.740065.000064.260071.300075.100072.6100
M4528.000028.260027.740070.000069.260076.950080.800078.2600
M4830.000030.260029.740075.000074.260082.600086.600083.9100
M5233.000033.210032.690080.000079.260088.300092.400089.5600
M5635.000035.310034.690085.000084.130093.630098.100095.0700
M6038.000038.310037.690090.000089.130099.3500103.9000100.7200
M6440.000040.310039.690095.000094.1300104.9800109.7000106.3700
M6843.000043.310042.6900100.000099.1300110.5000115.5000112.0200
M7245.0000  105.0000102.8000116.0300  
M7648.0000  110.0000107.8000121.5500  
M8050.0000  115.0000 127.3000  
M9057.0000  130.0000 144.0000  
M10063.0000  145.0000 161.0000  
M11069.0000  155.0000 171.2800  
M12579.0000  180.0000 198.9000  
M14088.0000  200.0000 221.0000  
M160100.0000  230.0000 254.1500  

 

 Metric Coarse Hexagon Head Bolt Grade-12.9 DIN931

Metric Coarse Hexagon Head Bolt CAP  high Grade CLASS 12.9 DIN 931

Additional Info
Additional Info
Weight0.0000
MaterialGrade-12.9
Standard NumberDIN931
Second Standard-
DriveHexagon
HeadHEXAGON
American Generic Brand TermHEXAGONCAP
Diameter M5,M6,M7,M8,M10,M12,M14,M16,M18,M20,M22,M24,M27,M30,M33,M36,M39,M42,M45,M48,M52,M56,M60,M64,M68,M72,M76,M80,M90,M100,M110,M125,M140,M160
Length6,8,10,12,14,16,18,20,22,24,26,28,30,35,40,45,50,55,60,65,70,75,80,85,90,95,100,110,120,130,140,150,160,170,180,190,200,210,220,230,240,250,260,270,280,300,320,340,350,360,380,400,420,440,460,480,500