Metric Coarse Flange Bolt Grade-12.9 DIN6921

SKU: 70
Details
Details
Metric Coarse Flange Bolt Grade-12.9 DIN6921
dkdc maxdc mines maxb L ? 125b 125 < L ? 200b L > 200l minl max
M55.800011.58009.80008.71008.000016.0000--10.000050.0000
M66.600014.200012.200010.950010.000018.0000--12.000060.0000
M88.100018.000015.800014.260013.000022.000028.0000-16.000080.0000
M109.200022.300019.600016.490015.000026.000032.0000-20.0000100.0000
M1211.500026.600023.800017.600016.000030.000036.0000-25.0000120.0000
M1412.800030.000027.600019.760018.000034.000040.0000-30.0000140.0000
M1614.400035.000031.900023.120021.000038.000044.000057.000035.0000160.0000
M2017.100043.000040.000028.500027.000046.000052.000065.000040.0000180.0000
Additional Info
Additional Info
Weight0.0000
MaterialGrade-12.9
Standard NumberDIN6921
Second StandardB18.2.3M
DriveHexagon
HeadFlange
American Generic Brand Term-
Diameter M5,M6,M8,M10,M12,M14,M16,M20
Length10,12,16,20,25,30,35,40,50,60,80,100,120,140,160,180