Inch Round Hammer Drive Screw 'U' Copper BS4174

SKU: 502
Details
Details
Inch Round Hammer Drive Screw 'U' Copper BS4174
dno. threadD maxD minA maxA minH maxH minP maxP mindrillhole
No.006.00000.06000.05700.09900.09000.03400.02600.04900.046055.00000.0520
No.06.00000.07500.07200.12700.11800.04900.04100.06300.060051.00000.0670
No.28.00000.10000.09700.16200.14600.06900.05900.08300.080044.00000.0860
No.47.00000.11600.11200.21100.19300.08600.07500.09600.092037.00000.1040
No.67.00000.14000.13600.26000.24000.10300.09100.11600.112031.00000.1200
No.78.00000.15400.15000.28500.26400.11100.09900.12600.122029.00000.1360
No.88.00000.16700.16200.30900.28700.12000.10700.13600.132027.00000.1440
No.108.00000.18200.17700.35900.33400.13700.12300.15000.146020.00000.1610
No.128.00000.21200.20600.40800.38200.15300.13900.17700.173011.00000.1910
No.149.00000.24200.23600.45700.42900.17000.15500.20200.19802.00000.2210
Additional Info
Additional Info
Weight0.0000
MaterialCOPPER
Standard NumberBS4174
Second Standard-
DriveNon
HeadROUND
American Generic Brand Term-
Diameter No.00,No.0,No.2,No.4,No.6,No.7,No.8,No.10,No.12,No.14
Length1/8",3/16",1/4",5/16",3/8",1/2",5/8",3/4",1"
Reviews
Tags
Tags