BSP Sealing Washer Copper DIN7603C

SKU: 1556
Details
Details
BSP Sealing Washer Copper DIN7603C
Dd1 d2h
1/4"0.26500.375020g
1/4"0.26500.437020g
1/4"0.26500.500020g
5/16"0.32300.437020g
5/16"0.32300.500020g
1/8"(3/8)   .3900.590020g
1/8"(3/8)   .3900.590018g
1/4"  .5300.720020g
1/4"  .5300.750018g
3/8"(21/32) .6650.875018g
1/2"(13/16) .8301.000018g
1/2"(13/16) .8301.040018g
5/8"(29/32) .9101.130016g
3/4"1.05001.320016g            
7/8"1.20001.500016g            
1"(1.5/16) 1.32 X1.620016g            
Additional Info
Additional Info
Weight0.0000
MaterialCOPPER
Standard NumberDIN7603C
Second Standard-
DriveNon
HeadNON
American Generic Brand Term-
Diameter 1/4",5/16",1/8",1/4",3/8",1/2",5/8",3/4",7/8",1"
LengthNON