Metric Coarse Captive Washer For DIN7964 Items Stainless-Steel-A2

SKU: 1597
Details
Details
Metric Coarse Captive Washer For DIN7964 Items Stainless-Steel-A2
dd1 mind2sb maxc min
M44.100019.50000.40003.80002.7000
M55.100020.50000.50004.00002.7000
M66.100021.50000.60004.20002.7000
M88.100025.00000.80005.40002.7000
M1010.100027.50001.00005.80002.7000
M1212.100029.50001.20006.50002.7000
Additional Info
Additional Info
Weight0.0000
MaterialStainless-Steel-A2
Standard Number.
Second Standard-
DriveNon
HeadNON
American Generic Brand TermWAISTED
Diameter M4,M5,M6,M8,M10,M12,M14,M16