84.20000.20000.4500
105.20000.25000.5500
12.56.20000.35000.8000
147.20000.35000.8000
168.20000.40000.9000
189.20000.45001.0500
2010.20000.50001.1500
22.511.20000.60001.4000
2512.20000.70001.6000
2814.20000.80001.8000
31.516.30000.80001.8500
35.518.30000.90002.0500
4020.40001.00002.3000
4522.40001.25002.8500
5025.40001.25002.8500
5628.50001.50003.4500
6331.00001.80004.1500
7136.00002.00004.6000
8041.00002.25005.2000
9046.00002.50005.7000
10051.00002.70006.2000
11257.00003.20007.2000
12564.00003.50008.5000
14072.00004.00009.0000
16082.00004.500010.5000
18092.00005.100011.1000
200102.00005.600013.6000
225112.00006.500014.5000
250127.00007.000017.0000
Additional Info
Additional Info
Weight0.0000
MaterialStainless-Steel
Standard NumberDIN2093A
Second Standard-
DriveNon
HeadNON
American Generic Brand Term BELLEVILLE,DISCSPRING
Diameter 8,10,12.5,14,16,18,20,22.5,25,28,31.5,35.5,40,45,50,56,63,71,80,90,100,112,125,140,160,180,200,225,250
LengthNON
Reviews
Tags
Tags

Use spaces to separate tags. Use single quotes (') for phrases.