D nom1/4”5/16”3/8”1/2”5/8”3/4”7/8”1.1/8”1.1/4”
D nom0.25000.31200.37500.50000.62500.75001.00001.25001.5000
D13/16”1/4”5/16”3/8”1/2”5/8”3/4”7/8”1.1/8”
BSW24.000020.000018.000016.000012.000011.000010.00009.00008.0000
D max0.24800.31100.37300.49800.62300.74800.99801.24801.4980
D Min0.24600.30900.37100.49600.62100.74600.99601.24601.4960
A max0.37500.43800.56200.75000.87501.00001.31201.75002.1250
A min0.35700.41900.54300.72900.85300.97701.28701.72302.0950
H max0.18800.21900.25000.31200.37500.50000.62500.75001.0000
H min0.17700.20900.24000.30200.36500.49000.61000.73500.9800
S min0.15700.18300.20900.26200.31500.42100.52700.63300.8420
J1/8”5/32”3/16”1/4”5/16”3/8”1/2”5/8”7/8”
J0.12500.15600.18800.25000.31200.37500.50000.62500.8750
T min0.09400.11700.14100.18800.23400.28100.37500.46900.6560
M max0.01400.01700.02000.02600.03200.03900.05000.06000.0700
R min0.00900.01200.01500.02000.02400.03000.04000.05000.0600
K min0.22700.28900.35200.47700.60200.72700.97701.22701.4780
F max0.09300.09300.09300.09300.09300.09300.12500.12500.1250
G max0.14200.19300.24900.30400.41400.52100.63800.75000.9640
G min0.13300.18200.23700.29100.39700.50200.61600.72600.9340
I max0.08300.10000.11100.12500.15400.18200.20000.22200.2860
N max0.02300.02800.03100.03500.04200.05100.05500.06200.0720
N min0.01700.02200.02500.02900.03600.04500.04900.05600.0660
E max0.37500.43800.50000.62500.75000.87501.00001.12501.5000

 

BSW Whitworth Hexagon Socket Shoulder Screw Grade-X(12.9) BS2470 bs 2470

Additional Info
Additional Info
Weight0.0000
MaterialGrade-X(12.9)
Standard NumberBS2470
Second Standard-
DriveHexagonsocket
HeadCAP
American Generic Brand TermALLEN,STRIPPER
Diameter 1/4",5/16",3/8",7/16",1/2",9/16",5/8",3/4",7/8",1.",1.1/8",1.1/4",1.3/8",1.1/2",1.3/4",2.
Length1/4,5/16,3/8,7/16,1/2",5/8",3/4",7/8",1.",1.1/8",1.1/4",1.3/8",1.1/2",1.5/8",1.3/4",2.",2.1/4",2.3/8",2.1/2",2.3/4",3.",3.1/4",3.1/2",3.3/4",4.",4.1/4",4.1/2",4.3/4",5.",5.1/4",5.1/2",5.3/4",6.",6.1/2",7.",7.1/2",8.",8.1/2",9.",9.1/2",10
Reviews
Tags
Tags

Use spaces to separate tags. Use single quotes (') for phrases.