Ds maxs minL2 maxL2 minL2 nom mmL1 maxL1 minL1 mm
0.028"0.02800.02750.31200.12506.00001.31201.125031.0000
0.035"0.03500.03450.43800.25009.00001.31201.125031.0000
0.050"0.05000.04900.62500.438014.00001.75001.562042.0000
1/16"0.06250.06150.65600.469014.00001.84401.656044.0000
5/64"0.07810.07710.70300.516015.00001.96901.781048.0000
3/32"0.09370.09270.75000.562017.00002.09401.906051.0000
7/64"0.10940.10790.79700.609018.00002.21902.031054.0000
1/8"0.12500.12350.84400.656019.00002.34402.156057.0000
9/64"0.14060.13910.89100.703020.00002.46902.281060.0000
5/32"0.15620.15470.93800.750021.00002.59402.406064.0000
3/16"0.18750.18601.03100.844024.00002.84402.656070.0000
7/32"0.21870.21721.12500.938026.00003.09402.906076.0000
1/4"0.25000.24851.21901.031029.00003.34403.156083.0000
5/16"0.31250.31101.34401.156032.00003.84403.656095.0000
3/8"0.37500.37351.46901.281035.00004.34404.1560108.0000
7/16"0.43750.43551.59401.406038.00004.84404.6560121.0000
1/2"0.50000.49751.71901.531041.00005.34405.1560133.0000
9/16"0.56250.56001.84401.656044.00005.84405.6560146.0000
5/8"0.62500.62251.96901.781048.00006.34406.1560159.0000
3/4"0.75000.74702.21902.031054.00007.34407.1560184.0000
7/8"0.87500.87202.46902.281060.00008.34408.1560210.0000
1"1.00000.99702.71902.531067.00009.34409.1560235.0000
1.1/4"1.25001.24303.25002.750076.000011.500011.0000286.0000
1.1/2"1.50001.49303.75003.250089.000013.500013.0000337.0000
1.3/4"1.75001.74304.25003.7500102.000015.500015.0000387.0000
2"2.00001.99304.75004.2500114.000017.500017.0000438.0000

 

Inch Hexagon Keys Short Arm  Alloy Steel B18.3 wrench

Additional Info
Additional Info
Weight0.0000
MaterialALLOY STEEL
Standard NumberB18.3
Second Standard-
DriveHexagonsocket
HeadNON
American Generic Brand TermALLEN,KEY,WRENCH
Diameter 0.028",0.035",0.050",1/16",5/64",3/32",7/64",1/8",9/64",5/32",3/16",7/32",1/4",5/16",3/8",7/16",1/2",9/16",5/8",3/4",7/8",1",1.1/4",1.1/2",1.3/4",2"
LengthNON
Reviews
Tags
Tags

Use spaces to separate tags. Use single quotes (') for phrases.