Ds maxs minL2 maxL2 minL2 nom mmL1 maxL1 minL1 mm
0.028"0.02800.02750.31200.12506.00002.68802.500066.0000
0.035"0.03500.03450.43800.25009.00002.76602.578068.0000
0.050"0.05000.04900.62500.438014.00002.93802.750072.0000
1/16"0.06250.06150.65600.469014.00003.09402.906076.0000
5/64"0.07810.07710.70300.516015.00003.28103.094081.0000
3/32"0.09370.09270.75000.562017.00003.46903.281086.0000
7/64"0.10940.10790.79700.609018.00003.65603.469090.0000
1/8"0.12500.12350.84400.656019.00003.84403.656095.0000
9/64"0.14060.13910.89100.703020.00004.03103.8440100.0000
5/32"0.15620.15470.93800.750021.00004.21904.0310105.0000
3/16"0.18750.18601.03100.844024.00004.59404.4060114.0000
7/32"0.21870.21721.12500.938026.00004.96904.7810124.0000
1/4"0.25000.24851.21901.031029.00005.34405.1560133.0000
5/16"0.31250.31101.34401.156032.00006.09405.9060152.0000
3/8"0.37500.37351.46901.281035.00006.84406.6560171.0000
7/16"0.43750.43551.59401.406038.00007.59407.4060191.0000
1/2"0.50000.49751.71901.531041.00008.34408.1560210.0000
9/16"0.56250.56001.84401.656044.00009.09408.9060229.0000
5/8"0.62500.62251.96901.781048.00009.84409.6560248.0000
3/4"0.75000.74702.21902.031054.000011.344011.1560286.0000
7/8"0.87500.87202.46902.281060.000012.844012.6560324.0000
1"1.00000.99702.71902.531067.000014.344014.1560362.0000
1.1/4"1.25001.24303.25002.750076.0000   
1.1/2"1.50001.49303.75003.250089.0000   
1.3/4"1.75001.74304.25003.7500102.0000   
2"2.00001.99304.75004.2500114.0000   

 

Inch Hexagon Keys Long Arm Alloy Steel B18.3 wrench

Additional Info
Additional Info
Weight0.0000
MaterialALLOY STEEL
Standard NumberB18.3
Second Standard-
DriveHexagonsocket
HeadNON
American Generic Brand TermALLEN,KEY,WRENCH
Diameter 0.028",0.035",0.050",1/16",5/64",3/32",7/64",1/8",9/64",5/32",3/16",7/32",1/4",5/16",3/8",7/16",1/2",9/16",5/8",3/4",7/8",1",1.1/4",1.1/2",1.3/4",2"
LengthNON
Reviews
Tags
Tags

Use spaces to separate tags. Use single quotes (') for phrases.