dda maxdkkrrfl minl max
22.80004.00001.40001.60003.20008.000020.0000
2.53.30005.00001.70002.00004.000010.000030.0000
33.80006.00002.10002.40004.800010.000040.0000
3.54.30007.00002.35002.80005.600010.000045.0000
45.00008.00002.80003.20006.400012.000050.0000
4.55.50009.00003.10003.60007.200016.000060.0000
56.000010.00003.50004.00008.000016.000080.0000
5.56.600011.00003.80004.40008.800020.000080.0000
67.200012.00004.20004.80009.600040.000080.0000
78.200014.00004.90005.600011.200040.000080.0000
810.200016.00005.60006.400012.800040.000080.0000
Additional Info
Additional Info
Weight0.0000
MaterialSTEEL
Standard NumberDIN7996H
Second Standard-
DrivePhillips
HeadROUND
American Generic Brand Term-
Diameter 2,2.5,3,3.5,4,4.5,5,5.5,6,7,8