Inch Square Head Coach Screw Steel ASME, B18.2.1. 1996
Inch Square Head Coach Screw Steel
Diameter | D Max | D Min | F | H | Threads Per Inch | Thread Pitch |
1⁄2 | 0.515 | 0.482 | 3⁄4 | 11⁄32 | 6 | 0.167 |
5⁄8 | 0.642 | 0.605 | 15⁄16 | 27⁄64 | 5 | 0.200 |
3⁄4 | 0.768 | 0.729 | 11⁄8 | 1⁄2 | 41⁄2 | 0.222 |
7⁄8 | 0.895 | 0.852 | 15⁄16 | 37⁄64 | 4 | 0.250 |
1 | 1.022 | 0.976 | 11⁄2 | 43⁄64 | 31⁄2 | 0.286 |
11⁄8 | 1.149 | 1.098 | 111⁄16 | 3⁄4 | 31⁄4 | 0.308 |
11⁄4 | 1.277 | 1.223 | 17⁄8 | 27⁄32 | 31⁄4 | 0.308 |
13⁄8 | 1.404 | 1.346 | 21⁄16 | 29⁄32 | 3 | 0.333 |
11⁄2 | 1.531 | 1.469 | 21⁄4 | 1 | 3 | 0.333 |
Standard Thread Length
The minimum thread length for square lag screws shall be equal to half the nominal screw length plus 1/2″ or 6″, whichever is less. One should consider longer than standard thread
Inch Square Head Coach Screw Steel, lag bolt, lag screw
ASME B18.2.1 1996
Weight | 0.0000 |
---|---|
Material | STEEL |
Standard Number | . |
Second Standard | - |
Drive | - |
Head | - |
American Generic Brand Term | - |
Diameter | 0 |
Length | 0 |