Inch Hexagon Head Self Tapping Screw AB Case Hardened Steel BS4174
SKU:
490
Details
Details
Inch Hexagon Head Self Tapping Screw AB Case Hardened Steel BS4174
d | s max | s min | e max | e min | k max | k min |
---|
No.4 | 0.1870 | 0.1810 | 0.2160 | 0.2020 | 0.0800 | 0.0700 |
No.6 | 0.2500 | 0.2440 | 0.2890 | 0.2720 | 0.1100 | 0.0950 |
No.8 | 0.2500 | 0.2440 | 0.2890 | 0.2720 | 0.1150 | 0.1000 |
No.10 | 0.3120 | 0.3050 | 0.3610 | 0.3400 | 0.1200 | 0.1050 |
No.12 | 0.3120 | 0.3050 | 0.3610 | 0.3400 | 0.1550 | 0.1390 |
No.14 | 0.3750 | 0.3670 | 0.4330 | 0.4090 | 0.1900 | 0.1720 |
No.16 | 0.5000 | 0.4890 | 0.5770 | 0.5450 | 0.2300 | 0.2080 |
Additional Info
Additional InfoWeight | 0.0000 |
---|
Material | CASE HARDENED STEEL |
---|
Standard Number | BS4174 |
---|
Second Standard | - |
---|
Drive | Hexagon |
---|
Head | HEXAGON |
---|
American Generic Brand Term | - |
---|
Diameter | No.2,No.4,No.6,No.8,No.10,No.12,No.14,No.16 |
---|
Length | 1/4",5/16",3/8",7/16",1/2",5/8",3/4",1",1.1/4",1.1/2",1.3/4",2",2.1/4",2.1/2",3" |
---|