da maxl2 mindin 6902A hdin 6902A d2din 6902B hdin 6902B d2din 6904 hdin 6904 d2
M2.50.90004.00000.60006.00000.80008.00001.05007.0000
M31.00004.00000.60007.00000.80009.00001.05008.0000
M3.51.20006.00000.80008.00000.800011.00001.15008.0000
M2.51.40006.00000.80009.00001.000012.00001.65009.0000
M31.60006.00001.000010.00001.600015.00001.750011.0000
M3.52.00008.00001.600012.00001.600018.00002.000012.0000
M82.500010.00002.000016.00002.000024.00002.400015.0000
M103.000012.00002.500020.00002.500030.00002.600021.0000
Additional Info
Additional Info
Weight0.0000
MaterialGrade-5.8
Standard NumberDIN69002
Second StandardISO10644
DriveVarious
HeadVarious
American Generic Brand Term-
Diameter M2.5,M3,M3.5,M2.5,M3,M3.5,M8,M10
Length12,14,16,18,20,22,24,26,28,30,35,40,45,50