Metric Coarse 12 Point Socket Screw Stainless-Steel-A4 DIN34821

SKU: 658
Details
Details

Metric Coarse 12 Point Socket Screw Stainless-Steel-A4 DIN34821

Ddk maxdk mink maxk mint maxt mindrives
M610.00009.78006.00005.70003.40003.0000N87.4000
M813.000012.73008.00007.64004.48004.0000N109.8400
M1016.000015.730010.00009.64005.48005.0000N1211.7000
M1218.000017.730012.000011.57006.48006.0000N1413.5400
M1421.000020.670014.000013.57007.58007.0000N1615.9900
M1624.000023.670016.000015.57008.58008.0000N1817.1800

FOR ADDITIONAL DRIVE INFORMATION SEE DIN34824



Metric Coarse 12 Point Socket Screw Stainless  Steel A4 DIN 34821

Additional Info
Additional Info
Weight0.0000
MaterialStainless-Steel-A4
Standard NumberDIN34821
Second Standard-
Drive12point
HeadCHEESE
American Generic Brand TermCHEESE,INTERNALFERRY
Diameter M6,M8,M10,M12,M14,M16
Length16,18,20,22,24,26,28,30,35,40,45,50,55,60,65,70,75,80,85,90,95,100