Metric Coarse Slotted Raised Countersunk Machine Screw Brass DIN964
D dk maxk maxn min t min
M11.90000.60000.31000.4000
M1.22.30000.72000.36000.5000
M1.42.60000.84000.36000.5200
M1.63.00000.96000.46000.6500
M23.80001.20000.56000.8000
M2.54.70001.50000.66001.0000
M35.60001.65000.86001.2000
M3.56.50001.93000.86001.4000
M47.50002.20001.00001.6000
M59.20002.50001.20002.0000
M611.00003.00001.60002.4000
M814.50004.00002.00003.2000
M1018.00005.00002.50004.0000
Additional Info
Additional Info
Weight0.0000
MaterialBRASS
Standard NumberDIN964
Second StandardISO2010
DriveSlot
HeadRaisedcountersunk
American Generic Brand TermFLAT
Diameter M1,M1.2,M1.4,M1.6,M2,M2.3,M2.5,M2.6,M3,M3.5,M4,M5,M6,M8,M10
Length2,3,4,5,6,8,10,12,14,16,18,20,22,24,26,28,30,35,40,45,50,55,60