UNC Phillips Binding Head Machine Screw Grade-4.8 B18.6.3

SKU: 408
Details
Details

UNC Phillips Binding Head Machine Screw Grade-4.8 B18.6.3


dNo. 2No.4No.6No.8No.101/4"
A Max0.1810.2350.2900.3440.3990.525
A Min0.1710.2230.2750.3260.3780.498
O Max0.0500.0680.0870.1050.1230.165
O Min0.0430.0610.0780.0950.1120.152
F Max0.0180.0250.0320.0390.0450.061
F Min0.0130.0180.0240.0290.0340.046
M Max0.1000.1180.1600.1860.2050.281
M Min0.0870.1050.1470.1730.1920.268
G Max0.0580.0770.0880.1140.1340.164
G Min0.0410.0590.0640.0900.1090.140
N Min0.0170.0170.0260.0280.0290.046
Driver112223

 

UNC Phillips Binding Head Machine Screw Grade CLASS 4.8  4.6 B18.6.3

Additional Info
Additional Info
Weight0.0000
MaterialGrade-4.8
Standard NumberB18.6.3
Second Standard-
Drive-
Head-
American Generic Brand Term-
Diameter0
Length0