Metric Fine Vargal Locking Nut Standard Class-8

SKU: 1002
Details
Details

Metric Fine Vargal Locking Nut Standard Class-8

dPitchshm
M6     0.75      10     8.2      4.5      
M8 1  13  10.8  6.7 
M12 1.125  19  16  10.6 
M12 1.5  19  16  10.6 
M10 1.25  17  12.6  8 
M14 1.5  22  18  12 
M16 1.5  24  20.6  13.5 
M18 1.5  27  22.5  14.5 
M22 1.5  32  29.8  20.5 
M20 1.5  30  25.5  16.9 
M24 2  36  29.9  20.6 
M27 2  41  33.7  24.3 
M30 2  46  37  26.6 
M33 2  50  40.5  28.8 
M36 3  55  44.2  31.5 

 

 

Metric Fine Vargal Lock Nut fastener Standard Class-8 class 8 grade 8 abbott jeveka etra kpo gally

Additional Info
Additional Info
Weight0.0000
MaterialClass-8
Standard Number.
Second StandardVARGAL
DriveHexagon
HeadNON
American Generic Brand Term STIFF, PREVAILING TORQUE