Metric Coarse Philidas Industrial Full Class-8

SKU: 945
Details
Details

Metric Coarse Philidas Industrial Full Class-8

 

DABC
M58.00006.50004.3000
M610.00007.50005.0000
M813.00008.50005.7000
M1017.000011.00008.0000
M1219.000013.00009.5000
M1422.000015.000011.0000
M1624.000017.000012.8000
M1827.000020.000015.5000
M2030.000022.000017.5000
M2232.000023.000018.0000
M2436.000025.000019.5000
M2741.000028.000022.0000
M3046.000031.000024.5000
M3350.000033.000026.2000
M3655.000036.000028.6000
M3960.000039.000031.1000
M4265.000042.000033.5000
M4570.000045.000036.0000
M4875.000048.000038.0000
M5280.000052.000041.5000

 

Metric Coarse Philidas Industrial Full grade Class-8 self-locking lock nut, Philidas Nut

Additional Info
Additional Info
Weight0.0000
MaterialClass-8
Standard Number.
Second StandardPHILIDAS
DriveHexagon
HeadNON
American Generic Brand Term STIFF, PREVAILING TORQUE
Diameter M5,M6,M8,M10,M12,M14,M16,M18,M20,M22,M24,M27,M30,M33,M36,M39,M42,M45,M48,M52
LengthNON