Details

 

        D             S             h
M35.50003.2000
M47.00003.2000
M58.00004.1000
M610.00006.1000
M813.00006.4000
M1017.00007.9000
M1219.00009.9000
M1422.000011.0000
M1624.000013.0000
M1827.000015.0000
M2030.000016.0000
M2232.000017.8000
M2436.000018.8000
M2741.000022.2000
M3046.000023.9000
M3655.000032.0000

 

 