BA Aerotight All Metal Locking Nut Thick Stainless-Steel-A4

SKU: 994
Details
Details

 

de maxn maxh maxf min
0BA0.41300.40300.32800.1880
2BA0.32400.31400.25600.1420
4BA0.24800.23800.20300.1100
6BA0.19300.18300.15700.0800

 

 

BA Aero tight All Metal Locking Nut Thick Stainless Steel A4

Additional Info
Additional Info
Weight0.0000
MaterialStainless-Steel-A4
Standard Number.
Second StandardAEROTIGHT
DriveHexagon
HeadNON
American Generic Brand Term STIFF, PREVAILING TORQUE
Diameter 0BA,2BA,4BA,6BA
LengthNON
Reviews
Tags
Tags

Use spaces to separate tags. Use single quotes (') for phrases.