BA Aerotight All Metal Locking Nut Thick Steel

SKU: 974
Details
Details

BA Aerotight All Metal Locking Nut Thick Steel

de maxn maxh maxf min
0BA0.41300.40300.32800.1880
2BA0.32400.31400.25600.1420
4BA0.24800.23800.20300.1100
6BA0.19300.18300.15700.0800

 

 

BA Aero tight All Metal Lock ing Nut Thick Steel

Additional Info
Additional Info
Weight0.0000
MaterialSTEEL
Standard Number.
Second StandardAEROTIGHT
DriveHexagon
HeadNON
American Generic Brand Term STIFF, PREVAILING TORQUE
Diameter 0BA,2BA,4BA,6BA
LengthNON