Metric Coarse Shear Nut Stainless-Steel

SKU: 1241
Details
Details
SIZEAFBCD
M6  10.00  10.00    0.50     6.00
M8  13.00  13.00    0.50     7.00
M10  17.00  17.00    1.00     9.00
M12  19.00  19.00    1.00  10.00
M16  24.00  24.00    1.50  14.00
M20  30.00  30.00    2.80  18.00

Metric Coarse Shear Nut Stainless-Steel

Additional Info
Additional Info
Weight0.0000
MaterialStainless-Steel
Standard Number.
Second StandardWS9305
Drive-
HeadHEXAGON
American Generic Brand Term-
Diameter0
LengthNON