UNC 12 Point Allen Nuts Stainless-Steel

SKU: 1243
Details
Details
UNC 12 Point Allen Nuts Stainless-Steel
db maxb minL maxL mind maxd mine nomf ming min
No.40.18700.18300.17900.17200.20900.20501/8”0.08000.0460
No.50.18700.18300.20500.19800.20900.20501/8”0.09500.0560
No.60.25700.25300.23000.22300.27800.27405/32”0.10000.0710
No.80.28000.27500.27300.26600.30700.30203/16”0.12500.0840
No.100.30700.30200.31900.30900.33600.33103/16”0.17000.0960
1/4”0.40300.39800.41900.40900.43000.42501/4”0.22500.1360
5/16”0.49800.49300.52200.51200.52600.52105/16”0.28500.1650
3/8”0.59000.58500.62100.60600.62000.61503/8”0.32500.1950
7/16”0.71000.70500.73300.71800.74300.73807/16”0.36000.2350
1/2”0.80000.79500.83600.82100.84100.83601/2”0.44500.2650
5/8”0.98600.98001.01000.99501.04001.03405/8”0.50000.3250
3/4”1.15801.15201.18501.17001.21501.20903/4”0.60000.3850
7/8”1.36101.35501.35801.34301.43001.42407/8”0.70000.4450
1”1.53301.52701.53201.51701.62001.61201”0.81000.4950
Additional Info
Additional Info
Weight0.0000
MaterialStainless-Steel
Standard Number.
Second Standard-
DriveNon
HeadNON
American Generic Brand TermALLEN
Diameter No4,No5,No6,No8,No10,1/4",5/16",3/8",7/16",1/2",5/8",3/4",7/8",1"
LengthNON