BSF Hexagon Lock Nut Thicker 3 Sizes Grade-A-Steel BS1083

SKU: 834
Details
Details
BSF Hexagon Lock Nut Thicker 3 Sizes Grade-A-Steel BS1083
d e s max s min m max m min
1/4"0.51000.44500.43800.16100.1510
5/16"0.61000.52500.51800.19300.1820
3/8"0.69000.60000.59200.22400.2140
Additional Info
Additional Info
Weight0.0000
MaterialGrade-A-Steel
Standard NumberBS1083
Second Standard-
DriveHexagon
HeadNON
American Generic Brand TermHALFNUT,JAMNUT
Diameter 1/4",5/16",3/8"