UNC Hexagon Collar Nut Steel

SKU: 1256
Details
Details
UNC Hexagon Collar Nut Steel
d1msd2a
No.105/16"3/8"1/2"1/16"
1/4"5/16"1/2"5/8"1/16"
5/16"3/8"9/16"3/4"1/16"
3/8"1/2"11/16"7/8"1/8"
7/16"9/16"3/4"15/16"1/8"
1/2"11/16"7/8"1.1/8"5/32"
5/8"13/16"1.1/16"1.3/8"3/16"
3/4"1"1.1/4"1.5/8"1/4"
7/8"1.1/8"1.7/16"1.3/4"1/4"
1"1.1/4"1.5/8"2"1/4"
1.1/8"1.3/8"1.13/16"2.1/4"1/4"
1.1/4"1.3/8"1.13/16"2.1/4"1/4"
1.1/2"1.1/2"2.3/16"2.3/4"1/4"
Additional Info
Additional Info
Weight0.0000
MaterialSTEEL
Standard Number.
Second Standard-
DriveHexagon
HeadNON
American Generic Brand Term-
Diameter No.10,1/4",5/16",3/8",7/16",1/2",5/8",3/4",7/8",1",1 1/8",1 1/4",1 1/2"