dtypeABCDEGH
No. 10Light1.31000.48000.29000.47000.65000.08000.1200
No. 10Regular1.40000.53000.25000.50000.75000.08000.1400
No. 12Regular1.28000.40000.23000.59000.73000.11000.1200
1/4"Light1.28000.40000.23000.59000.73000.11000.1200
1/4"Regular1.78000.66000.31000.70001.03000.14000.1700
1/4"Heavy1.47000.50000.37000.66001.03000.14000.1400
5/16"Regular1.78000.66000.31000.70001.03000.14000.1700
5/16"Heavy1.47000.50000.37000.66001.03000.14000.1400