Metric Coarse Engineers Stud Metal End =2 D Interferance Fit Grade-10.9 DIN949A
d b c l<125 c l<125<200 c l 200>
MFS 510.000016.000022.0000 
MFS 612.000018.000024.000037.0000
MFS 714.000020.000026.000039.0000
MFS 816.000022.000028.000041.0000
MFS 1020.000026.000032.000045.0000
MFS 1224.000030.000036.000049.0000
MFS 1428.000034.000040.000053.0000
MFS 1632.000038.000044.000057.0000
Additional Info
Additional Info
Weight0.0000
MaterialGrade-10.9
Standard NumberDIN949A
Second Standard-
DriveNon
HeadNON
American Generic Brand Term-
Diameter MFS5,MFS6,MFS7,MFS8,MFS10,MFS12,MFS14,MFS16
Length22,25,30,35,40,45,50,55,60,65,70,75,80,85,90,95,100,110,120,130,140,150,160