Metric Coarse Square Neck Tee Slot Bolt Stainless-Steel-A2 DIN186B

SKU: 201
Details
Details
Metric Coarse Square Neck Tee Slot Bolt Stainless-Steel-A2 DIN186B
d b k n e max
M618.00004.50006.000016.9000
M822.00005.50008.000018.9000
M1026.00007.000010.000022.0000
M1230.00008.000012.000027.0000
M1638.000010.500016.000031.0000
M2046.000013.000020.000037.2500
M2454.000015.000024.000044.2500
M3066.000019.000030.000055.5000
M3678.000023.000036.000067.5000
M4296.000026.000042.000081.5000
M48108.000030.000048.000089.7500
Additional Info
Additional Info
Weight0.0000
MaterialStainless-Steel-A2
Standard NumberDIN186B
Second Standard-
DriveNon
HeadTEE
American Generic Brand TermT'
Diameter M6,M8,M10,M12,M16,M20,M24,M30,M36,M42,M48
Length30,35,40,45,50,55,60,65,70,75,80,85,90,95,100,110,120,130,140,150,160,170,180,190,200