BSW Whitworth Slotted Mushroom Head Machine Screw Grade-4.8 BS450

SKU: 2382
Details
Details
BSW Whitworth Slotted Mushroom Head Machine Screw Grade-4.8 BS450
dddk maxdk mink maxk minn maxn mint nom
1/8”0.12500.28900.27200.07800.06600.04300.03500.0400
3/16”0.18750.44800.42500.11800.10300.06000.05000.0610
1/4”0.25000.57300.54600.15000.13300.07500.06400.0790
5/16”0.31250.69800.66600.18300.16200.08400.07200.0960
3/8”0.37500.82300.78700.21500.19100.09400.08100.1120
Additional Info
Additional Info
Weight0.0000
MaterialGrade-4.8
Standard NumberBS450
Second Standard-
DriveSlot
HeadMushroom
American Generic Brand Term TRUSS,SHALLOW PAN, MUSHROOM
Diameter 1/8”,3/16”,7/32”,1/4”,5/16”,3/8”
Length1/8"3/16",1/4",5/16",3/8",1/2",5/8",3/4",7/8",1.",1.1/8",1.1/4",1.3/8",1.1/2",1.5/8",1.3/4",2.",2.1/4",2.3/8",2.1/2",2.3/4",3.",3.1/4",3.1/2",3.3/4",4.",4.1/4",4.1/2",4.3/4",5."