de maxn maxh maxf min
3/16”0.32400.31400.21200.0980
1/4”0.44500.43300.24500.1080
5/16”0.52500.51300.29900.1410
3/8”0.60000.58800.35500.1830
1/2”0.82000.80800.47500.2660

 

 

British Standard Whitworth b.s.w. Aero tight All Metal Lock ing Nut Thin Stainless Steel A4

Additional Info
Additional Info
Weight0.0000
MaterialStainless-Steel-A4
Standard Number.
Second StandardAEROTIGHT
DriveHexagon
HeadNON
American Generic Brand Term STIFF, PREVAILING TORQUE
Diameter 3/16",1/4",5/16",3/8",1/2"